词条 | Palmqvist method | ||||||||||||||||||
释义 |
The Palmqvist method, or the Palmqvist toughness test, (after Sven Robert Palmqvist) is a common method to determine the fracture toughness for cemented carbides. In this case, the materials fracture toughness is represented by the critical stress intensity factor KIC.[2] ApproachThe Palmqvist-method uses the lengths of the cracks from a number of Vickers indentions to determine the fracture toughness.[2] The critical stress intensity factor is then given by: with the unit . Notes1. ^S. Palmqvist, Occurrence of crack formation during Vickers indentation as a measure of the toughness of hard materials, Arch Eisenhuettenwes, 33 (1962) 629-333. 2. ^1 Detta är hårdmetall {{webarchive|url=https://web.archive.org/web/20160127040808/http://www2.sandvik.com/sandvik/0130/HI/SE03411.nsf/7a5364adb7735b05412568c70034ea1b/4c7827530abfa4e1c1256b0a0034cc36/%24FILE/ATT7Q52S/9100 |date=2016-01-27 }}, Digital compendium - Sandvik, (in Swedish), Retrieved 22 January 2016 1 : Materials testing |
||||||||||||||||||
随便看 |
|
开放百科全书收录14589846条英语、德语、日语等多语种百科知识,基本涵盖了大多数领域的百科知识,是一部内容自由、开放的电子版国际百科全书。